Arcaloy® 309L-16 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700 deg F (370 deg C). Post weld heat treatment should only be performed after due consideration.
Products specifications
| Product type | Consumable |
| Length | 12 |
| Chemical Composition | C/Mn/Si/Ni/Cr/Mo/Cu/Ferrite FN |
| Container Size | 10 |
| Container Type | Sealed Can |
| Diameter | 3/32 |
| Tensile Strength | 450 |